| Επισημαίνω: | 1600 °C Max Working Temperature SNSiC Kiln Beams,High-Temperature SNSiC Kiln Beams,Structural Integrity Silicon Carbide Beams |
||
|---|---|---|---|
| Material Type | Max Working Temperature | Key Properties | Best Suited for Kiln Furniture? |
|---|---|---|---|
| Sintered SiC (SNSiC/SSiC) | Up to 1600 °C | High Strength, Excellent Corrosion & Oxidation Resistance, Low Porosity | ✅ YES - Ideal for high-load, long-life beams and supports |
| Recrystallized SiC (RSiC) | Up to 1600°C | High Thermal Shock Resistance, Porous Structure | ⚠️ LIMITED - Excellent for tiles, but lower strength than SNSiC for heavy beams |
| Nitride-Bonded SiC (NSiC) | Up to 1450°C | Good Oxidation Resistance, Cost-Effective | ⚠️ LIMITED - Lower temperature ceiling and strength than SNSiC |
| Silicon-Infiltrated SiC (SiSiC) | Up to 1350°C | High Thermal Shock Resistance | ❌ NO - Lower maximum temperature limit |
| Property | Unit | Value (SNSiC) | Benefit for Your Kiln |
|---|---|---|---|
| Main Composition | % | >99% SiC | Ensures purity and superior high-temperature performance |
| Bulk Density | g/cm³ | 3.0 - 3.1 | High density translates to exceptional mechanical strength and load capacity |
| Porosity | Vol-% | < 5% | Extremely low porosity prevents gas infiltration, enhancing oxidation resistance and longevity |
| Flexural Strength | MPa | 370 - 420 | Outstanding resistance to bending and fracture under heavy loads at temperature |
| Thermal Conductivity | W/(m*K) | ~125 | Promotes rapid, even heat distribution, reducing firing times and improving energy efficiency |
| Max Use Temperature | °C | 1600 | Future-proofs your kiln for a wide range of ceramics and firing schedules |