Product Details:
|
| Material: | SiC | Composition:SiC: | >85% |
|---|---|---|---|
| Color: | Black | Density: | ≥3.65g/cm3 |
| Max. Service Temp: | 1380℃ | Flexural Strength: | 250MPa |
| Hardness: | ≥84HRA | Water Absorption: | ≤0.2% |
| Abrasion: | < 0.02% | Bending Strength: | ≥290MPa |
| Highlight: | 99.9% Aluminum Oxide Ceramics,Aluminum Oxide Ceramics 260MPa,99.9% Al2O3 Ceramics |
||
| Unit | Value |
|---|---|
| Density (g/cm³) | 3.9 |
| Compressive Strength (MPa) | 2500 |
| Tensile Strength (MPa) | 260 |
| Flexural Strength @ 20°C (MPa) | 350 |
| Flexural Strength @ 800°C (MPa) | 250 |
| Fracture Toughness KIc (MPa m^1/2) | 4.5 |
| Young's Modulus E (GPa) | 350 |
| Poisson Ratio | 0.22 |
| Hardness Knoop (1000g) (GPa) | 14 |
| Unit | Value |
|---|---|
| Maximum Temperature (°C) | 1700 |
| Thermal Conductivity @ 20°C (W/mK) | 28 |
| Thermal Expansion a at 20-100°C (10-6/K) | 8.4 |
| Specific Heat 100°C | 880 |
| Thermal Shock Parameter R1 (K) | 200 |
| Unit | Value |
|---|---|
| Dielectric Constant (1 MHz) | 9.7 |
| Dielectric Strength (6.35mm) (ac-kV/mm) | 8.7 |
| Dielectric Loss (tan delta 25° C) (1 MHz) | 0.0001 |
| Volume Resistivity @ 25°C (Ωcm) | 10^14 |
| Volume Resistivity @ 500°C (Ωcm) | 2x10^10 |
| Volume Resistivity @ 1000°C (Ωcm) | 2x10^6 |
Contact Person: Ms. Yuki
Tel: 8615517781293