Product Details:
|
| Material: | Silicon Nitride | Composition:SiC: | >85% |
|---|---|---|---|
| Color: | Black | Density: | 3.20-3.26g/cm3 |
| Max. Service Temp: | 1450℃ | Flexural Strength: | 250MPa |
| Sample: | Customizable | Chemical Stability: | High |
| Apparent Porosity: | 0-0.1% | Elastic Modulus: | 300-320GPa |
| Compression Strength: | >1500MPa | Vickers Hardness(HV0.5): | 15-16GPa |
| Thermal Conductivity: | 20-25W/(m.k) | Specific Resistivity: | 10^14Ω·cm |
| Highlight: | Si3N4 Silicon Nitride Ceramics,OEM Silicon Nitride Ceramics,Black Si3N4 Ceramics |
||
| Category | Property | Unit | 99% Al₂O₃ | S-SiC | ZrO₂ | Si₃N₄ |
|---|---|---|---|---|---|---|
| Physical | Density | g/cm³ | 3.9 | 3.1 | 6.0 | 3.2 |
| Water Absorption | % | 0 | 0.1 | 0 | 0.1 | |
| Physical | Sintering Temperature | °C | 1700 | 2200 | 1500 | 1800 |
| Mechanical | Hardness (HV) | HV | 1700 | 2200 | 1300 | 1400 |
| Flexural Strength | kgf/mm² | 3500 | 4000 | 9000 | 7000 | |
| Mechanical | Compressive Strength | kgf/mm² | 30000 | 20000 | 20000 | 23000 |
| Thermal | Max Working Temperature | °C | 1500 | 1600 | 1300 | 1400 |
| Thermal Expansion Coefficient (0-1000°C) | /°C | 8.0 * 10⁻⁶ | 4.1 * 10⁻⁶ (0-500°C) | 9.5 * 10⁻⁶ | 2.0 * 10⁻⁶ (0-500°C) | |
| 5.2 * 10⁻⁶ (500-1000°C) | 4.0 * 10⁻⁶ (500-1000°C) | |||||
| Thermal Shock Resistance | ΔT (°C) | 200 | 250 | 300 | 400-500 | |
| Thermal Conductivity (25°C) | W/m*K | 31 | 100 | 3 | 25 | |
| Thermal | Thermal Conductivity (300°C) | W/m*K | 16 | 100 | 3 | 25 |
| Electrical | Volume Resistivity (20°C) | Ω*cm | >10¹² | 10⁶-10⁸ | >10¹⁰ | >10¹¹ |
| Volume Resistivity (100°C) | Ω*cm | 10¹²-10¹³ | - | - | >10¹¹ | |
| Volume Resistivity (300°C) | Ω*cm | >10¹² | - | - | >10¹¹ | |
| Dielectric Breakdown Strength | kV/mm | 18 | Semiconductor | 9 | 17.7 | |
| Dielectric Constant (1 MHz) | ε | 10 | - | 29 | 7 | |
| Dielectric Loss Tangent | tan δ | 0.4 * 10⁻³ | - | - | - |
Contact Person: Ms. Yuki
Tel: 8615517781293