Product Details:
|
| Main Ingredients: | Al2O3+ZrO2+SiO2+others | Color: | White Or Yellowish |
|---|---|---|---|
| Density: | ≥3.70 G/cm³ | Bulk Density: | ≥2.20 G/cm³ |
| Vickers Hardness HV5: | 1350 Kg/mm2 | Sphericity: | >95% |
| Highlight: | Toughened Zirconia Ceramic Beads,Wear Resistant Zirconia Ceramic Beads,Ultra Hard Zirconia Milling Media |
||
Our K-380 Zirconia Toughened Alumina (ZTA) Beads are high-performance composite ceramic grinding media engineered for high-speed and high-energy milling processes, such as agitator and sand mills. They deliver exceptional wear resistance and grinding efficiency for a wide range of hard-to-grind materials.
| Specification | K-380 Beads |
|---|---|
| Density | ≥ 3.70 g/cm³ |
| Bulk Density | ≥ 2.20 g/cm³ |
| Vickers Hardness (HV5) | 1350 kg/mm² |
| Sphericity | > 95% |
| Size Range | 0.3 - 20.0 mm |
| Main Composition | Al₂O₃, ZrO₂, SiO₂ |
| Color | White / Yellowish |
Contact Person: Ms. Yuki
Tel: 8615517781293